FERRIT MAGNETER
Kontakt
+45 46 35 17 88
hindsbo@magneter.dk
Lokation
Byleddet 2,
4000 Roskilde
Menu
BM1
|
BM3
|
BM5
|
BM7
|
BM8
|
|||||
Remance
|
Br
|
210-220
|
350-370
|
390-400
|
350-370
|
380-390
|
mTesla
|
||
Coercivity
|
HcB
|
130-135
|
155-175
|
145-160
|
210-245
|
|
kA/m
|
||
Pol. Coercivity
|
HcJ
|
210-220
|
160-180
|
150-165
|
220-255
|
245-265
|
kA/m
|
||
Max. BH product
|
(BH)max
|
7.2-7.6
|
24-25.5
|
28-29.5
|
24.5-25.5
|
26-27.8
|
kj/m3
|
||
Curie point
|
–
|
450
|
450
|
450
|
450
|
450
|
°C
|
||
Max. operating temp.
|
–
|
250
|
250
|
250
|
250
|
250
|
°C
|
||
Temp. coeff. of Br
(-40 – +20°C)
|
–
|
-0.2
|
-0.2
|
-0.2
|
-0.2
|
-0.2
|
%/C
|
||
Temp. coeff of HcJ
(-40 – +200°C)
|
–
|
0.4
|
0.4
|
0.4
|
0.4
|
0.4
|
%/C
|
||
Density
|
–
|
4.9
|
4.8
|
4.9
|
4.65
|
4.8
|
g/cm3
|
||
Barium/Strontium
|
B
|
B
|
B
|
S
|
S
|
||||
Isotropic/Anisotropic
|
I
|
A
|
A
|
A
|
A
|
Se råmagnet oversigt:Tryk her